Sign In | Join Free | My himfr.com |
|
Ask Lasest Price | |
Brand Name : | oem odm |
Price : | Negotiated |
Payment Terms : | T/T |
Supply Ability : | 10000PCS |
Delivery Time : | 20 days after 2D 3D confirmed |
PEEK is difficult to meet the different requirements of different industries and fields. Therefore, in special working environment, PEEK needs to be modified by mainly means of blending modification, copolymerization modification, composite reinforcement modification, filling modification, nano modification and surface modification. The modification can increase some aspects of PEEK, such as wear resistance and impact strength, so as to expand the application scope of PEEK, reduce the cost of materials and improve the processing performance of PEEK.
Modified PEEK
Glass fiber modification: 10% glass fiber modification, 20% glass fiber modification, 30% glass fiber modification
Carbon fiber modification: 10% carbon fiber modification, 20% carbon fiber modification, 30% carbon fiber modification.
VALUE | UNIT | TEST | |
Gravity (23°C) | 1.28 ~ 1.38 | g/cm3 | ASTM D792 |
1.26 ~ 1.38 | g/cm3 | ISO 1183 | |
Melt flow rate (400°C/2.16 kg) | 2.0 ~ 36 | g/10 min | ASTM D1238 |
MVR (380°C/10.0 kg) | 14.1 ~ 23.8 | cm3/10min | ISO 1133 |
![]() |